Behaviour of oxygen in CZ-silicon during 430–630°C heat
treatment
Om Prakash, N.K Upreti
1
, Shyam Singh *
Department of Physics, G.B. Pant Uni6ersity of Ag. and Tech., Pantnagar 263 145, India
Received 23 July 1997; accepted 14 October 1997
Abstract
The generation of thermal donors (TDs) depends on initial oxygen concentration, annealing temperature and its duration. An
annealing process at 450°C for several hours generates upto :1016
cm3
TDs. We found that maximum concentration of TDs
formed at 480°C was :1.01015
cm3
which reduces to a minimum of :2.61014
cm3
at 510°C suggesting thereby that the
TDs got annihilated in this temperature range. The number of TDs now increases with a corresponding increase in annealing time
giving birth to new donors (NDs). Activation energy for oxygen diffusion was found to be 0.690.1 eV and of silicon self
interstitials :0.4 eV. Therefore, it is quite logical to conclude that oxygen diffusion at low temperatures depends on the transport
of the self interstitials which are chiefly due to the formation of molecule-like oxygen clusters. This confirms the formation and
diffusion of molecule-like oxygen clusters in silicon at low temperatures. © 1998 Elsevier Science S.A. All rights reserved.
Keywords: Thermal donors; New donors; Thermal acceptor; Kinetics; Dimers; Activation energy

Behaviour of oxygen in CZ-silicon during 430–630°C heat treatment.pdf

116.51 KB, 下载次数: 1

您需要登录后才可以回帖 登录 | 立即注册

本版积分规则

投诉/建议联系

爆料/投稿:8328 6054 @qq.com

举报/投诉:刘先生/158 5085 4264(微信同号) 商务/合作:夏 云/151 8971 7421(微信同号) 未经授权禁止转载,复制和建立镜像,
如有违反,追究法律责任
  • 阳匠学社
    微信公众号
  • 阳匠网
    微信公众号
阳匠网丨社区 © 2001-2025 Discuz! Team. Powered by Discuz! W1.5 苏ICP备2023010470号
关灯 在本版发帖
扫一扫添加微信客服
返回顶部
快速回复 返回顶部 返回列表